What all exactly will you we doing? This will help us to help you with quantities needed. You'll want to get a Un-waxed Ortho Laminating Polyester Resin. You'll also want to get Cabosil, and some 1/4" chopped Milled Strand. If you want to make your own Faring material some Glass Bubbles will be needed as well.
Hey woody, long time no hear.......I've been away from home for nearly a year and have since moved lock stock and barrel over a thousand miles to my current location.
So I've found a supplier for all the f\glass components and some bits and pieces. They can supply me with 20mm honeycomb composite panels for all the structural components, stringers, deck, bulkheads and transom at nearly the same cost as marine ply.
Here is the list I'm putting together
3 x 20 litre unwaxed ortho vinylester and catalyst
roll of csm (what weight is best for light structural repairs and waterproofing?)
How much 1708 (or equivalent) strong structural repairs like stringers, decking and transom.
I'll get a number of 1 litre (or so) of as pots for resin during the wetting out of the glass.
Stirrers rollers gloves clamps (all hail nurseman!) etc.
Cabosil for PB and loose glass.
Am i missing much?
As always your help is greatly appreciated.
Cheers from The Darling Downs in Queensland!