GCartwright
Petty Officer 2nd Class
Thread starter- Joined
- Jul 1, 2012
- Messages
- 149
The deck is down using pl and stainless screws, all sections are glassed with csm on the bottom, seams are all filled and tabbed, two layers of 1708 between the deck and hull, foaming is finished, about a litre left over from the 10 gallon kit, had one classic over pour episode,
Next is two layers of csm and one layer of 6 oz with wax on the top layer since I'm going with carpeting
Next is two layers of csm and one layer of 6 oz with wax on the top layer since I'm going with carpeting