My aluminum hull is showing some pitting along the waterline where the paint is coming off. Also a little is showing up on the bottom. I plan on adding some zinc anodes to the hull.
What is a good way to clean the corrosion (white stuff) before I paint again?

Yes I use this boat in saltwater. I will be rewiring too as we believe there was some stray current.
 

Bondo

Moderator
Staff member
Joined
Apr 17, 2002
Messages
71,539
Re: Galvanic corrosion problem

What is a good way to clean the corrosion (white stuff) before I paint again?

Ayuh,.....

The same way we clean aluminum for welding,...... With a SSteel wirebrush.....
A SSteel cup brush on a 4" grinder will make Quick work of it......;)
 

Pursuit2150

Chief Petty Officer
Joined
Dec 3, 2001
Messages
553
Re: Galvanic corrosion problem

Before you paint,clean the area well, polish the areas with 000 steel wool..
Spray the area with ,Zinc-Chromate primer then Top coat.
 

Redneck

Seaman
Thread starter
Joined
Oct 7, 2007
Messages
51
Re: Galvanic corrosion problem

Thanks, what should I use to clean it with? I have heard water with baking soda.
 