So, I was in over my head on how much time I had to spend on this boat and sold it to another sick individual who shared the love for fine, old tin boats. I'm working on another boat, a 1983 Lund vhull, also aluminum, and I have some corrosion repair from wet foam to do. Does anyone mind if I ask some tin hull repair questions here for the Lund? These scenarios are all below waterline. I plan to use Marinetex to fill pits on the inside, but while waiting for that stuff to ship, will the JB weld I have on hand be ok to get started? For pits that have gone through the hull, can I fill them with the either product with a piece of tape on the outside, then sand outside after it cures? Is a rivet ever warranted in the corrosion hole? Im using Gluvit (on the way) for seams and rivets; does it go right over the epoxy repair (once cured)? I read not to use a steel wire wheel to remove corrosion, but then what do I use? The brass wire wheels for the Dremel are only 3/4" diameter, and they're the only pure brass wire wheels I can find. All others seem to be either SS or brass-coated steel, which seems like it'd wear off in no time and you'd be using plain steel anyway.