Could post in Props, but think better response here. 12 weeks in the salt pond. New zinc at the prop, motor zinc was wire brushed to a good polish and replaced. All bolts had no antisieze for good contact. Prop/LU have been Primered and TriLux'ed. The back end had the usual crud on it, the lower powerwashed off fine, but the prop looks like crap. This year I even tried leaving 3 or 4 splines grease free for a good contact. Heres what it looks like. Any opinions? Thanks..